Getting light out of high-index LED chips
Micro-LED chips are made of GaN (n ≈ 2.4). A bare chip surface reflects 17 % straight back even at normal incidence, and in a flat stack only light within 24.6° of the normal can ever reach the air. Stepping the index down in layers cuts the reflection losses; a high-index layer with a shaped surface — a microlens or texture — accepts a much wider cone from the chip and lets it out. An AR-coated cover keeps ambient reflections down.
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (8)
- Anti-reflection coating Low index n 1.16–1.40 or multi-layer ARK1
- Cover glass n 1.52
- Optical fill / adhesive Not Kriya
- Colour-conversion layer Quantum dots on blue LEDs (in colour-converted designs)
- High-index extraction layer Graded n 1.95 → 1.40, or imprinted high-index microlenses / textureK2
- Micro-LED chips GaN · n ≈ 2.4
- TFT backplane Not Kriya
- Substrate Glass or silicon
Referenzen
- Numerical analysis of high-index nanocomposite encapsulant for light-emitting diodes — arXiv:physics/0511010
Zugehörige Kriya-Seiten
- kriya-materials.com/applications/displays
- kriya-materials.com/applications/nanoimprint-wafer-level-optics
Hier verwendete Kriya-Werkzeuge
Schematisch, nicht maßstabsgetreu.