Beleuchtung

Edge-lit glass light panel

Luminous glass for buildings, furniture and signage

A glass pane lit from its edge glows wherever an extraction pattern sends the light out. As soon as the pane is laminated, bonded or held by a material of similar index, the light escapes there instead. A low-index coating on the glass keeps the light guided — and lets the panel be laminated into safety glass or bonded into a frame.

FRONTBACKCover glass (optional)Laminated or bondedInterlayer or adhesivePVB, EVA or OCA · n ≈ 1.48 · not KriyaLow-index coatingKeeps the light in the guideLight-guide glass with edge LEDsLow-iron glass · n 1.52Extraction patternPrint, etch or laserReflector or back glass (optional)Not KriyaK1
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (6)
  1. Cover glass (optional) Laminated or bonded
  2. Interlayer or adhesive PVB, EVA or OCA · n ≈ 1.48 · not Kriya
  3. Low-index coating Keeps the light in the guideK1
  4. Light-guide glass with edge LEDs Low-iron glass · n 1.52
  5. Extraction pattern Print, etch or laser
  6. Reflector or back glass (optional) Not Kriya

Referenzen

  1. US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
  2. EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder

Schematisch, nicht maßstabsgetreu.