Energie, Gebäude & Landwirtschaft
Greenhouse glazing
More light for the crop through the same glass
At higher latitudes, natural light limits crop growth in greenhouses through autumn and winter. Each bare glass surface reflects 4.3 % at normal incidence — about 8 % for the two faces of a pane — before the light reaches the crop. Anti-reflection on both faces recovers most of that, and an anti-soiling top coat helps keep the roof clean.
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (4)
- Anti-soiling top coat Outer faceK2
- Anti-reflection, outer face Porous low-index layerK1
- Greenhouse glass Clear or diffuse, ≈ 4 mm · n 1.52
- Anti-reflection, inner face Porous low-index layerK1
Referenzen
- F. Kempkes et al., Increase of light transmission by 10% in the Venlo-type greenhouse: from design to results of a cucumber experiment — Acta Horticulturae 1296 (2020): diffuse glass with an anti-reflective coating among the measures; light transmission increased by more than 10 %
- New glass coatings for high insulating greenhouses without light losses — energy saving, crop production and economic potentials — Acta Horticulturae 893 (ISHS): anti-reflection coatings on greenhouse glass