Rechenzentrum & Photonik

Co-packaged optics

Polymer waveguides between photonic chip and fibre

Co-packaged optics moves the optical engine next to the switch chip. Polymer waveguides on the package carry light between the photonic chip and the fibres and couple adiabatically to silicon-nitride waveguides on the chip. They are built like a coating stack — lower cladding, core, upper cladding — and cured with UV and heat, so the index of every layer has to be set precisely.

TOP SIDEPACKAGEUpper claddingLow indexWaveguide coresPatterned by lithography or imprintLower claddingLow indexPhotonic chip with SiN tapersCoupling region: tapers under the polymercores · not KriyaPackage substrate or interposerNot KriyaK1K2K1
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (5)
  1. Upper cladding Low indexK1
  2. Waveguide cores Patterned by lithography or imprintK2
  3. Lower cladding Low indexK1
  4. Photonic chip with SiN tapers Coupling region: tapers under the polymer cores · not Kriya
  5. Package substrate or interposer Not Kriya

Referenzen

  1. J. Van Asch et al., Low-Loss Integration of High-Density Polymer Waveguides with Silicon Photonics for Co-Packaged Optics — arXiv:2503.02712 (2025): adiabatic coupling between on-chip SiN and package-level polymer waveguides
  2. Y. Shen et al., Polymer Waveguides for Co-Packaged Optics — precise refractive-index control between core and cladding; propagation loss < 0.1 dB/cm at 850 nm
  3. Silicon photonics packaging with single-mode polymer waveguides — process: lower cladding, core, patterning, upper cladding; UV and thermal cure

Schematisch, nicht maßstabsgetreu.