AR glasses — diffractive waveguide
A small projector injects the image into a high-index glass plate. An imprinted in-coupling grating bends the light into total internal reflection; fold and out-coupling gratings spread it across the eye box and send it to the eye. The gratings are fragile, every interface costs light, and the plate can only guide the angles its index contrast allows — which sets the field of view.
Vollständige Schichtliste (8)
- Hard coat, AR and easy-clean On the world-side cover lensK1
- World-side protective lens Polycarbonate or glass
- Low-index encapsulation Over the gratings; allows bonding and stackingK3
- Nanoimprinted gratings In-coupler, fold and out-coupler · high-index resinK2
- Waveguide plate High-index glass n ≈ 1.7–2.0 · ≈ 0.5–1 mm
- Low-index bonding layer Between stacked plates (RGB stacks use 1–3 plates)K3
- Eye-side protective or prescription lens Polymer or glass
- Hard coat and multi-layer AR Eye sideK1
Arbeitsweise
Version 1 · erstmals veröffentlichtGratings imprinted in a high-index resin, a low-index layer over them and between stacked plates, coated cover lenses behind air gaps.
Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.
- Imprint the gratings
UV nanoimprint resin with an index at or near that of the plate: solvent-free resins up to n 1.65, imprint-proven up to n 1.79. A resin that matches the plate leaves no reflecting boundary under the gratings.
Schichten: Nanoimprinted gratings - Cover the gratings with a low-index layer
Hollow-silica coating without PFAS, n 1.16–1.40, overcoatable, at least 1 µm thick: ten times the reach of the evanescent field (about 0.1 µm).
Schichten: Low-index encapsulation - Stack the plates on low-index layers
The same layer between the plates of an RGB stack: each plate keeps guiding, and there is no air gap to keep clean and sealed.
Schichten: Low-index bonding layer - Coat the cover lenses
Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry. The covers stay behind air gaps.
Schichten: Hard coat, AR and easy-clean · Hard coat and multi-layer AR
Öffentliche Grundlage
Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.
- M. Burghoorn et al., Improving the efficiency of copper indium gallium (di-)selenide (CIGS) solar cells through integration of a moth-eye textured resist with a refractive index similar to aluminum doped zinc oxide — 2014, open access: a texture imprinted in a resist whose index is close to that of the layer under it.
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001: a low-index coating made of fine hollow particles in a binder.
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000: a layer bonded to a light guide through a lower-index layer; guided light is totally reflected at that interface.
Bleibt beim Gerätehersteller
Grating design, plate glass, the number of plates and the way a prescription is added.
Diese Beschreibung ist kein juristischer Hinweis.
Referenzen
- B. Kress, Optical waveguide combiners for AR headsets: features and limitations — Proc. SPIE 11062, 110620J (2019)
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
- M. Burghoorn et al., Improving the efficiency of copper indium gallium (di-)selenide (CIGS) solar cells through integration of a moth-eye textured resist with a refractive index similar to aluminum doped zinc oxide — AIP Advances 4, 127154 (2014), open access
Zugehörige Kriya-Seiten
- kriya-materials.com/applications/ar-vr-waveguides
- kriya-materials.com/applications/nanoimprint-wafer-level-optics
Hier verwendete Kriya-Werkzeuge
Schematisch, nicht maßstabsgetreu.