AR headset — curved visor combiner

Displays above the eyes, image reflected by the visor

The simplest see-through display projects the image from displays above the eyes onto a large curved visor. A semi-reflective coating on the inside of the visor sends the image to the eyes; the outside surface sends a second, shifted copy. On a visor this ghost is strong: the mirror is weak, so most of the light reaches the outer surface.

WORLD SIDEEYE SIDEEasy-clean top layerOuter faceHard coat and AR, outer faceConvex side of the visorPolycarbonate visorInjection-moulded · n 1.59Semi-reflective coatingEven thickness over the inner face · about40 % · vacuum dielectric stack, not KriyaAirDisplays and lenses above the eyesNot KriyaK2K1
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (5)
  1. Easy-clean top layer Outer faceK2
  2. Hard coat and AR, outer face Convex side of the visorK1
  3. Polycarbonate visor Injection-moulded · n 1.59
  4. Semi-reflective coating Even thickness over the inner face · about 40 % · vacuum dielectric stack, not Kriya
  5. Displays and lenses above the eyes Not Kriya

Arbeitsweise

Version 1 · erstmals veröffentlicht

Hard coat, AR and easy-clean on the outer face; one mirror of even thickness on the inner face.

Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.

  1. Hard coat with AR on the outer face

    Hard coat 3H+ to 4H; two-layer UV-curable AR on polycarbonate, high index ≈ 1.75 under low index ≈ 1.30. Behind a 40 % mirror the ghost falls from 4.6 % of the image to 0.9 % at R = 1 % and 0.14 % at R < 0.15 %.

    Schichten: Hard coat and AR, outer face
  2. Easy-clean top layer

    Water contact angle above 100° without fluorinated chemistry.

    Schichten: Easy-clean top layer
  3. Mirror of even thickness on the inner face

    Vacuum coating over the whole face, about 40 %. Not Kriya.

    Schichten: Semi-reflective coating

Öffentliche Grundlage

Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.

Bleibt beim Gerätehersteller

Mirror design and reflectance, visor shape and display optics.

Diese Beschreibung ist kein juristischer Hinweis.

Referenzen

  1. US 3,870,405 — Helmet sight visors — 1975 patent: visor with a partially reflective inner surface; the ghost image comes from the outer surface
  2. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids