AR glasses — reflective waveguide
A reflective waveguide carries the image inside a glass plate by total internal reflection and couples it out with a row of embedded, partially reflective surfaces. The plate guides only while its faces meet something of much lower index. Bond a cover plate straight onto it and the image leaks into the cover. A low-index coating between plate and cover keeps the light guided without an air gap; the lower its index, the more field of view survives.
Vollständige Schichtliste (9)
- Hard coat, AR and easy-clean On the world-side coverK1
- World-side cover plate Flat glass or polymer · n ≈ 1.5
- Optical adhesive Not Kriya
- Low-index layer A few µm · n ≈ 1.2–1.25K2
- Glass waveguide with partial mirrors n ≈ 1.5–1.8 · embedded reflective surfaces · not Kriya
- Low-index layer A few µm · n ≈ 1.2–1.25K2
- Optical adhesive Not Kriya
- Eye-side cover plate Flat · a prescription lens stays a separate part
- Hard coat and multi-layer AR Eye sideK1
Arbeitsweise
Version 1 · erstmals veröffentlichtA low-index layer on both guiding faces, flat cover plates bonded over it, coated outer faces.
Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.
- Coat both guiding faces with a low-index layer
n 1.20–1.25, 1 µm or more: a ray 5° beyond the critical angle reaches only about 0.1 µm into the layer. Against n 1.20 an n 1.60 plate guides beyond 48.6°.
Schichten: Low-index layer - Bond flat cover plates over it
With the low-index layer in between, the index of the adhesive no longer matters. Adhesive and covers are not Kriya.
Schichten: Optical adhesive · World-side cover plate · Eye-side cover plate - Coat the outer faces
Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.
Schichten: Hard coat, AR and easy-clean · Hard coat and multi-layer AR
Öffentliche Grundlage
Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000: a layer bonded to a light guide through a lower-index layer; guided light is totally reflected at that interface.
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001: a low-index coating made of fine hollow particles in a binder.
Bleibt beim Gerätehersteller
The plate with its partial mirrors, the coupling prism, and the prescription lens, which stays a separate part.
Diese Beschreibung ist kein juristischer Hinweis.
Referenzen
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder
Zugehörige Kriya-Seiten
Hier verwendete Kriya-Werkzeuge
Schematisch, nicht maßstabsgetreu.