AR & VR

AR projector — micro-LED light engine

Pixels, micro-lenses and projection lens in a few cubic millimetres

The projector of AR glasses has to fit into a temple a few millimetres wide. A micro-LED panel sends its light into a wide cone, but the projection lens accepts only a narrow one: an F/2 lens takes about 6 % of the light of a flat emitter. A micro-lens on every pixel narrows the cone before the light is lost, and every lens surface after that needs an anti-reflection coating.

TO THE WAVEGUIDEBACKPLANEAR on the projection lens surfacesEvery element, both facesProjection lens groupMoulded or wafer-level lensesAirLow-index cap over the micro-lensesFlat, closed surfaceMicro-lens arrayOne lens per pixel · imprinted high-indexresinMicro-LED pixelsGaN, n ≈ 2.4 · pitch of a few µm · not KriyaCMOS backplaneNot KriyaK2K3K1
Veröffentlichte Kriya-PositionPassgenaue Kriya-PositionWeitere Schicht
Vollständige Schichtliste (6)
  1. AR on the projection lens surfaces Every element, both facesK2
  2. Projection lens group Moulded or wafer-level lenses
  3. Low-index cap over the micro-lenses Flat, closed surfaceK3
  4. Micro-lens array One lens per pixel · imprinted high-index resinK1
  5. Micro-LED pixels GaN, n ≈ 2.4 · pitch of a few µm · not Kriya
  6. CMOS backplane Not Kriya

Arbeitsweise

Version 1 · erstmals veröffentlicht

A micro-lens per pixel imprinted in a high-index resin, a flat low-index cap, anti-reflection on the projection lens.

Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.

  1. Imprint the micro-lens array

    UV nanoimprint resin, one lens per pixel: solvent-free resins up to n 1.65, imprint-proven up to n 1.79.

    Schichten: Micro-lens array
  2. Flat low-index cap over the lenses

    The lower the index of the cap, the more lens power remains: under an n 1.50 planarisation an n 1.79 lens keeps 37 % of its power, under n 1.20 75 %.

    Schichten: Low-index cap over the micro-lenses
  3. AR on every projection lens surface

    Multi-layer AR, R < 0.15 %.

    Schichten: AR on the projection lens surfaces

Öffentliche Grundlage

Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.

Bleibt beim Gerätehersteller

Micro-LED pixels, backplane and projection optics.

Diese Beschreibung ist kein juristischer Hinweis.

Referenzen

  1. H. W. Choi et al., GaN micro-light-emitting diode arrays with monolithically integrated sapphire microlenses — Appl. Phys. Lett. 84, 2253 (2004): one micro-lens per micro-LED emitter
  2. US 5,479,049 — Solid state image sensor provided with a transparent resin layer having water repellency and oil repellency and flattening a surface thereof — 1995 patent: flat resin layer with an index below that of the micro-lenses, over the lens array of an image sensor
  3. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids

Schematisch, nicht maßstabsgetreu.