A holographic waveguide couples light in and out with volume gratings recorded in a photopolymer or liquid-crystal layer only a few micrometres thick. The substrates around it can be thin glass or plastic of ordinary index, so the range of guided angles is narrow from the start. Every layer added outside the guide — a cover, a second colour plate, a laminate — has to be separated from it by something of very low index.
Vollständige Schichtliste (9)
- Hard coat, AR and easy-clean On the world-side coverK1
- World-side cover Bonded with optical adhesive · not Kriya
- Low-index layer 0.5–2 µm · n ≈ 1.2K2
- Substrate Glass or polymer, 50–500 µm · n ≈ 1.52
- Holographic grating layer Photopolymer or liquid-crystal polymer, 2–5 µm · not Kriya
- Substrate Glass or polymer
- Low-index layer 0.5–2 µm · n ≈ 1.2K2
- Eye-side cover plate Bonded with optical adhesive · not Kriya
- Hard coat and multi-layer AR Eye sideK1
Arbeitsweise
Version 1 · erstmals veröffentlichtA low-index layer on both outer faces of the guide, flat covers bonded over it, coated outer faces.
Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.
- Coat both outer faces of the guide with a low-index layer
n about 1.2, 0.5–2 µm. Against n 1.20 an n 1.52 guide guides beyond 52.1°. For polymer substrates: n 1.21 with an 80 °C cure, UV-curable from n 1.30.
Schichten: Low-index layer - Bond flat covers over it
Optical adhesive on the low-index layer. Adhesive and covers are not Kriya.
Schichten: World-side cover · Eye-side cover plate - Coat the outer faces
Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.
Schichten: Hard coat, AR and easy-clean · Hard coat and multi-layer AR
Öffentliche Grundlage
Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000: a layer bonded to a light guide through a lower-index layer; guided light is totally reflected at that interface.
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001: a low-index coating made of fine hollow particles in a binder.
Bleibt beim Gerätehersteller
The grating layer, its recording and the layout of the guide.
Diese Beschreibung ist kein juristischer Hinweis.
Referenzen
- B. Kress, Optical waveguide combiners for AR headsets: features and limitations — Proc. SPIE 11062, 110620J (2019)
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
- EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder
Zugehörige Kriya-Seiten
Hier verwendete Kriya-Werkzeuge
Schematisch, nicht maßstabsgetreu.