AR glasses — freeform prism
A freeform prism folds the image inside a single moulded wedge. The light enters through one surface, is totally reflected at the eye-side surface, reflected again at the half-mirrored outer surface and then leaves through the same eye-side surface it was just reflected from. A second lens cemented to the outside restores the undistorted view of the world. The eye-side surface therefore has two jobs — mirror for steep rays, window for the rest — and it is the surface the wearer can touch.
Vollständige Schichtliste (8)
- Hard coat and AR, world side On the auxiliary lensK1
- Auxiliary (compensator) lens Corrects the see-through view
- Optical cement Not Kriya
- Half-mirror on the prism's outer surface Not Kriya
- Free-form prism PMMA (n 1.49) or cyclo-olefin (n 1.53)
- Coating on the eye-side surface Reflects by total internal reflection and transmitsK2
- AR on the display-side entry surfaceK3
- Micro-display Not Kriya
Arbeitsweise
Version 1 · erstmals veröffentlichtHard coat and AR on the auxiliary lens, AR on the entry surface, an easy-clean layer on the surface that reflects by total internal reflection.
Wie diese Beschichtung aufgetragen wird — Schritte, öffentliche Grundlagen, und was beim Gerätehersteller bleibt.
- Hard coat and AR on the auxiliary lens
Hard coat 3H+ to 4H with multi-layer AR, R < 0.15 %, on the world side.
Schichten: Hard coat and AR, world side - AR on the entry surface
Single low-index layer, n 1.30, about 106 nm: about 0.5 % luminous reflectance on PMMA instead of 3.9 % (thin-film model).
Schichten: AR on the display-side entry surface - Easy-clean layer on the eye-side surface
A transparent coating leaves total internal reflection where it is, from 42.2°; a fingerprint (n ≈ 1.47) would move that limit to 80.6°. Water contact angle above 100° without fluorinated chemistry.
Schichten: Coating on the eye-side surface
Öffentliche Grundlage
Ausgewählte abgelaufene Patente, erschienene Arbeiten, Bücher und Normen, die den Stand der Technik beschreiben.
- US 5,701,202 — Head or face mounted image display apparatus — 1995: three-surface prism whose eye-side surface both totally reflects and transmits, with a see-through element cemented on.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
Bleibt beim Gerätehersteller
Prism shape, half-mirror and display.
Diese Beschreibung ist kein juristischer Hinweis.
Referenzen
- US 5,701,202 — Head or face mounted image display apparatus — 1995 filing: three-surface prism whose eye-side surface both totally reflects and transmits; see-through element cemented on
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids