Head-up display
A HUD reflects an image off the windshield into the driver's view. Conventional HUDs use the s-polarised reflection from the inner glass surface and hide the second reflection, from the outer surface, with a wedge-shaped interlayer. p-polarised HUDs project close to the Brewster angle (≈ 57° for glass), where bare glass reflects little p-light, and use a reflecting layer inside the laminate instead. In both, the image leaves the HUD unit through a cover in the dashboard.
All layers (6)
- Outer glass n 1.52
- PVB interlayer n 1.48 · wedge-shaped for the HUD · ATO-loaded for solar controlK1
- Inner glass n 1.52
- HUD cover lens Polycarbonate or glass · closes the dashboard apertureK2
- Aspheric and fold mirrors Not Kriya
- Picture-generation unit TFT-LCD, micromirror or laser scanner
Public references
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
More on kriya-materials.com
- kriya-materials.com/applications/automotive-optics
- kriya-materials.com/applications/automotive-thermal
Kriya tools used on this page
Schematic, not to scale. Layer order, indices and thicknesses are typical values from the public references; real devices differ by maker and generation. Kriya values as published on kriya-materials.com. Kriya formulates every coating for the customer's substrate, process and specification.