跨行業驗證成果
与汽车OEM、显示器制造商、玻璃公司、太阳能集成商和光学公司实际合作的匿名化成果。每个数字均经实测研发数据和合作伙伴评估验证。
13
记录成果
6
应用领域
>500
全球服务企业
20年以上
历史记录
資料依據:
Displays
0.41%Haze (vs 0.68% incumbent)
ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser film
A leading Asian display film producer
Displays — Foldable200kFold cycles passed
Single-layer hardcoat passes 200,000 fold cycles with PFAS-free anti-smudge
A major Korean display Tier-1
Optical Components
8HPencil hardness at RI 1.85
Thermal HRI coating reaches RI > 1.8 and 8H pencil hardness on specialty glass
A specialty glass manufacturer
Architectural Glass4.5×Luminance improvement
LRI coating survives 630°C tempering, delivers 2.5–4.5× light guiding gain
A European glass industry leader
Automotive Thermal<0.3%Haze (automotive grade)
ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partner
A Tier-1 PVB interlayer manufacturer
Automotive Thermal−9°CCabin temperature reduction
Cabin temperature reduced by 9°C with ATO glazing integration
An Asian automotive OEM
Displays<0.15%Residual reflectance
Broadband reflectance below 0.15% achieved on multi-layer AR stack
A leading Tier-1 display optical film manufacturer
Automotive Thermal+16 kmRange extension (premium segment)
16 km additional EV range through solar heat control glazing
For an EV car model, a study was carried out
Solar & Energy+3.9%Transmission gain
3.9% transmission gain on photovoltaic cover glass with thermal-curable LRI
A leading solar module integrator
Displays — Scale500k kgTotal volume delivered
500,000 kg antistatic hardcoat supplied over 4 years as sole global supplier
A major Korean display OEM
Displays — ULR0.3×Reflection vs reference
ARAF nanoparticle composition achieves 0.3× reference reflection level
A leading Japanese AR film manufacturer
Displays — Foldable>100°Water contact angle (PFAS-free)
PFAS-free flexible AR achieves WCA >100° with better retention than PFAS
A major Korean display Tier-1
Automotive Thermal2,000 hrAccelerated weathering passed
ATO in PVB passes 2,000-hour accelerated weathering test
A Tier-1 PVB interlayer manufacturer
方法论
我们如何验证声明
本页面的每个指标均可追溯至实测研发数据、合作伙伴评估报告或客户现场验证。未经实验确认,我们不发布建模性能数据。
- 按ISO和ASTM标准测量的光学特性(透射率、雾度、反射率、WCA)
- 按ASTM D3359(附着力)、JIS K5600(铅笔硬度)的机械特性
- 按IEC 61215耐候性试验、客户指定折叠循环测试的耐久性
- 根据政策对客户名称匿名化。结构性描述已通过合规审批。
想成为我们的下一个案例?
我们与领先的OEM和集成商合作,在实际生产平台上验证涂层性能。