VOC-emissiecalculator

How much volatile organic content does this formulation release?

Schat jaarlijkse VOC-emissies en vergelijk met EU IED-drempels.

How it works

Volatile organic content of a coating formulation is the mass fraction of solvent that evaporates during cure. It is computed from the solvent mass balance of the as-applied wet formulation. Regulatory limits are stated in grams of VOC per litre of coating ready for application.

Worked example

50 % solids waterborne at 1.05 g/mL, 5 % exempt → 450 g/L VOC

EU VOC Directive 2004/42/EC calculation from solids, density and exempt fraction.

Validation method, references and test-case results: /validation#voc-calculator

Request accessOpen the interactive tool