TIR & Escape-Cone Calculator

How much light escapes the exit interface of a high-index medium?

Kritische hoek, ontsnapfractie, geleide fractie en de minimale manteldikte — voor de geometrie die u daadwerkelijk gebruikt, niet de leerboekvariant.

How it works

Light inside a high-index medium escapes into a lower-index external medium only within the escape cone set by the critical angle of total internal reflection. Isotropic emission inside the high-index medium puts a fixed fraction of its total power into that cone. The escaping fraction depends only on the two refractive indices.

Worked example

Critical angle, glass n 1.52 → air

Inputs: n1 = 1.52, n2 = 1

Result: 41.14 °

Reference: Born & Wolf §1.5.4

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#tir-escape-cone-calculator

Request accessOpen the interactive tool