Gevoeligheidsanalyse

Which layer thickness or index drives the design spec?

Bekijk welke laag in uw Multilayer thin-film stack de golflengte-opgeloste Reflectantie-gevoeligheid bepaalt.

How it works

The sensitivity of a stack's output metric to a layer parameter is the partial derivative of that metric with respect to the parameter at the nominal design. Finite-difference evaluation of the transfer-matrix forward model gives these derivatives directly. Ranking the layers by sensitivity identifies where the production tolerance budget most needs to be tight.

Worked example

Kriya 4-layer broadband, ∂R/∂n and ∂R/∂d

Per-layer ∂R/∂n and ∂R/∂d; central-difference Jacobian over the stack.

Validation method, references and test-case results: /validation#sensitivity

Request accessOpen the interactive tool