Multi-layer reverse engineering
What does a customer's reference coating appear to contain?
Identificeer een onbekende stack uit gemeten T(λ) en/of R(λ). Differential evolution over een door jou gekozen materialen-palet; top-3 kandidaat-stacks.
How it works
A reverse-engineering workflow combines non-destructive optical measurements (reflectance, transmittance, colour) with destructive chemical measurements (XPS, SIMS, FTIR) to constrain the likely stack architecture and materials of an unknown coating. The result is a hypothesis, not a proof — a candidate stack whose forward model matches the measurements.
Worked example
Planted 4-layer AR stack
Fit against a known planted stack; top-3 candidates ranked by residual MSE.
Validation method, references and test-case results: /validation#reverse-engineering