Brewster-hoek Calculator

At what angle does p-polarised reflection vanish for this interface?

Brewster-hoek en pseudo-Brewster-minimum voor elk grensvlak — polarisatie-discriminatie, complexe brekingsindex, kritische-hoek-regime, AR-ontwerp-context.

How it works

Brewster's angle is the angle of incidence at which p-polarised light is fully transmitted and only s-polarised light is reflected. For real media it is arctan(n2/n1); for absorbing or anisotropic media the exact minimum is called the pseudo-Brewster angle and shifts with the imaginary part of the refractive index.

Worked example

Brewster angle, air → n 1.52

Inputs: n1 = 1, n2 = 1.52

Result: 56.66 °

Reference: Hecht, Optics 5th ed. §4.7

Computed by this tool's kernel at build (commit dae6663).

Validation method, references and test-case results: /validation#brewster

Request accessOpen the interactive tool