Alle producten
KM-PSA-001PFAS-vrij verkrijgbaar
PFAS-Free Antistatic PSA
PFAS-free pressure-sensitive adhesive with integrated antistatic functionality. Designed for display panel lamination where both bonding and ESD protection are required in a single material.
Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-PSA
Specificaties
Functies
Pressure-sensitive adhesiveAntistatic
Compatibele substraten
PETGlass
Verwerkingsmethoden
SLOT DIER2R
Brekingsindex-bereik
1.48–1.55
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-PSA-001 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.48–1.55 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | Pressure-sensitive adhesive, Antistatic |
| Compatibele substraten | PET, Glass |
| Verwerking | SLOT DIE, R2R |
| Productblok | KM-PSA |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.