Alle producten
KM-700PFAS-vrij verkrijgbaar
HRI 100% Solids
Ultra-high RI 100% solids UV-curable formulation for waveguide core layers and metalens master-mold replication. NIL-compatible at R2R scale, enabling approximately 10× cost reduction versus wafer-based processing.
Brekingsindex-bereikn = 1.55–1.65
1.162.00
Chemiefamilie100% solids UV-curable
UithardingstypeUV
ProductblokKM-700–704
Specificaties
Functies
High RI
Compatibele substraten
PETGlass
Verwerkingsmethoden
R2RNILSLOT DIE
Brekingsindex-bereik
1.55–1.65
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-700 |
| Chemiefamilie | 100% solids UV-curable |
| Brekingsindex-bereik | 1.55–1.65 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | High RI |
| Compatibele substraten | PET, Glass |
| Verwerking | R2R, NIL, SLOT DIE |
| Productblok | KM-700–704 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.