Alle producten
KM-404PFAS-vrij verkrijgbaar
Add NIR to External Material
ATO nanoparticle dispersion additive that can be incorporated into third-party materials to add NIR absorption. Bottom-up synthesised with haze <0.3%. Compatible with PVB, PU, and other host matrices for automotive and architectural glazing.
Brekingsindex-bereikn = 0.00–0.00
1.162.00
ChemiefamilieSolvent sol-gel
UithardingstypeThermal
ProductblokKM-401–409
Specificaties
Functies
NIR absorbing
Compatibele substraten
PVBPUGlass
Verwerkingsmethoden
SPRAYDIP
Brekingsindex-bereik
0.00–0.00
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-404 |
| Chemiefamilie | Solvent sol-gel |
| Brekingsindex-bereik | 0.00–0.00 |
| Uithardingstype | Thermal |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | NIR absorbing |
| Compatibele substraten | PVB, PU, Glass |
| Verwerking | SPRAY, DIP |
| Productblok | KM-401–409 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Gerelateerde casestudies
Automotive Thermal<0.3%Haze (automotive grade)ATO dispersion achieves 0.2–0.3% haze in PVB, validated by Tier-1 interlayer partnerAutomotive Thermal−9°CCabin temperature reductionCabin temperature reduced by 9°C with ATO glazing integrationAutomotive Thermal+16 kmRange extension (premium segment)16 km additional EV range through solar heat control glazing
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.