Alle producten
KM-301PFAS-vrij verkrijgbaar
100% Solids HC
Solvent-free 100% solids UV-curable hard coating for high-throughput R2R and NIL processing. Zero VOC emissions. Enables precise nanostructure replication for waveguide gratings and metalens patterns.
Brekingsindex-bereikn = 1.50–1.55
1.162.00
Chemiefamilie100% solids UV-curable
UithardingstypeUV
ProductblokKM-301–309
Specificaties
Functies
Hard coating
Compatibele substraten
PETPCPMMAGlass
Verwerkingsmethoden
R2RNILSCREEN PRINTINGSLOT DIE
Brekingsindex-bereik
1.50–1.55
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-301 |
| Chemiefamilie | 100% solids UV-curable |
| Brekingsindex-bereik | 1.50–1.55 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | Hard coating |
| Compatibele substraten | PET, PC, PMMA, Glass |
| Verwerking | R2R, NIL, SCREEN PRINTING, SLOT DIE |
| Productblok | KM-301–309 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.