Alle producten
KM-203PFAS-vrij verkrijgbaar
Dual-Cure Antifouling
Dual-cure antifouling coating that achieves full cross-linking via combined UV and thermal cure. PFAS-free anti-smudge performance with WCA >100° on curved and complex substrates.
Brekingsindex-bereikn = 1.40–1.50
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeDual-cure
ProductblokKM-201–203
Specificaties
Functies
Antifouling
Compatibele substraten
PCPMMAGlass
Verwerkingsmethoden
SPINDIPSPRAY
Brekingsindex-bereik
1.40–1.50
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-203 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.40–1.50 |
| Uithardingstype | Dual-cure |
| PFAS-status | PFAS-vrij verkrijgbaar · fluorinated version available on request |
| Functies | Antifouling |
| Compatibele substraten | PC, PMMA, Glass |
| Verwerking | SPIN, DIP, SPRAY |
| Productblok | KM-201–203 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |