Alle producten
KM-107PFAS-vrij verkrijgbaar
Thermal AS AF
Dual-function thermal-curable coating combining antistatic and antifouling properties. Proven in foldable display applications with steel wool abrasion resistance exceeding 2,000 cycles while maintaining WCA above 95°.
Brekingsindex-bereikn = 1.45–1.50
1.162.00
ChemiefamilieThermal-curable latex
UithardingstypeThermal
ProductblokKM-101–140
Specificaties
Functies
AntistaticAntifouling
Compatibele substraten
PETPCGlass
Verwerkingsmethoden
SPINDIPROLLSPRAY
Brekingsindex-bereik
1.45–1.50
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-107 |
| Chemiefamilie | Thermal-curable latex |
| Brekingsindex-bereik | 1.45–1.50 |
| Uithardingstype | Thermal |
| PFAS-status | PFAS-vrij verkrijgbaar · fluorinated version available on request |
| Functies | Antistatic, Antifouling |
| Compatibele substraten | PET, PC, Glass |
| Verwerking | SPIN, DIP, ROLL, SPRAY |
| Productblok | KM-101–140 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.