Alle producten
KM-040PFAS-vrij verkrijgbaar
Multilayer Antireflection
Multi-layer anti-reflection stack utilising Kriya’s full RI platform (1.35–1.95) to achieve broadband residual reflectance below 0.15%. Validated on PET, PC, PMMA, and TAC substrates with transmission gains of 2–3.3%.
Brekingsindex-bereikn = 1.35–1.95
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeDual-cure
ProductblokKM-001–040
Specificaties
Functies
Anti-reflectiveMultilayer AR
Compatibele substraten
PETPCPMMATACGlass
Verwerkingsmethoden
SPINDIPROLLGRAVURESLOT DIE
Brekingsindex-bereik
1.35–1.95
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-040 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.35–1.95 |
| Uithardingstype | Dual-cure |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | Anti-reflective, Multilayer AR |
| Compatibele substraten | PET, PC, PMMA, TAC, Glass |
| Verwerking | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde casestudies
Displays0.41%Haze (vs 0.68% incumbent)ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser filmDisplays<0.15%Residual reflectanceBroadband reflectance below 0.15% achieved on multi-layer AR stackDisplays — ULR0.3×Reflection vs referenceARAF nanoparticle composition achieves 0.3× reference reflection level
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.