Alle producten
KM-035PFAS-vrij verkrijgbaar
AR + AF HC
Combined anti-reflective, antifouling, and hard coating in a UV-curable multi-layer or single-pot system. Addresses the three most common display surface requirements simultaneously.
Brekingsindex-bereikn = 1.35–1.60
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040
Specificaties
Functies
Anti-reflectiveAntifoulingHard coating
Compatibele substraten
PETPCPMMATAC
Verwerkingsmethoden
SPINDIPROLLGRAVURESLOT DIE
Brekingsindex-bereik
1.35–1.60
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-035 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.35–1.60 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar · fluorinated version available on request |
| Functies | Anti-reflective, Antifouling, Hard coating |
| Compatibele substraten | PET, PC, PMMA, TAC |
| Verwerking | SPIN, DIP, ROLL, GRAVURE, SLOT DIE |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.