Alle producten
KM-032PFAS-vrij verkrijgbaar

AS AF HC UV Weatherable

Four-function UV-curable coating: antistatic, antifouling, hard coating, and UV weatherability. Designed for demanding outdoor display applications that require multiple protective functions in minimal layers.

Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040

Specificaties

Functies

AntistaticAntifoulingHard coating

Compatibele substraten

PETPCPMMA

Verwerkingsmethoden

SPINDIPROLLGRAVURE

Brekingsindex-bereik

1.48–1.55
1.162.00
EigenschapWaarde
ProductcodeKM-032
ChemiefamilieSolvent UV-curable hybrid
Brekingsindex-bereik1.48–1.55
UithardingstypeUV
PFAS-statusPFAS-vrij verkrijgbaar · fluorinated version available on request
FunctiesAntistatic, Antifouling, Hard coating
Compatibele substratenPET, PC, PMMA
VerwerkingSPIN, DIP, ROLL, GRAVURE
ProductblokKM-001–040
BatchgroottesVanaf 40 kg monster tot productieschaal
Houdbaarheid6 maanden (ongeopend)
KwaliteitISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch.

Monster aanvragen

Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.

Neem contact op