Alle producten
KM-029PFAS-vrij verkrijgbaar
AG + AF HC
Multi-functional UV-curable coating combining anti-glare, antifouling, and hard coating in a single layer. Ideal for touch-panel displays and automotive interior surfaces.
Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040
Specificaties
Functies
Anti-glareAntifoulingHard coating
Compatibele substraten
PETPCPMMATAC
Verwerkingsmethoden
SPINDIPROLLGRAVURE
Brekingsindex-bereik
1.48–1.55
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-029 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.48–1.55 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar · fluorinated version available on request |
| Functies | Anti-glare, Antifouling, Hard coating |
| Compatibele substraten | PET, PC, PMMA, TAC |
| Verwerking | SPIN, DIP, ROLL, GRAVURE |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.