KM-027PFAS-vrij verkrijgbaar

AF + UV Weatherable HC

Triple-function UV-curable coating combining antifouling, hard coating, and UV weatherability. Designed for outdoor display and automotive applications requiring long-term durability against UV degradation and surface fouling.

Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040

Specificaties

Functies

AntifoulingHard coatingUV protection

Compatibele substraten

PETPCPMMA

Verwerkingsmethoden

SPINDIPROLLGRAVURE

Brekingsindex-bereik

1.48–1.55
1.162.00
EigenschapWaarde
ProductcodeKM-027
ChemiefamilieSolvent UV-curable hybrid
Brekingsindex-bereik1.48–1.55
UithardingstypeUV
PFAS-statusPFAS-vrij verkrijgbaar · fluorinated version available on request
FunctiesAntifouling, Hard coating, UV protection
Compatibele substratenPET, PC, PMMA
VerwerkingSPIN, DIP, ROLL, GRAVURE
ProductblokKM-001–040
BatchgroottesVanaf 40 kg monster tot productieschaal
Houdbaarheid6 maanden (ongeopend)
KwaliteitISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch.

Monster aanvragen

Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.