Alle producten
KM-015PFAS-vrij verkrijgbaar
1-Pot AS AF HC Thermal
Triple-function thermal-curable coating combining hard coating, antifouling, and antistatic properties. Eliminates three separate coating steps in a single formulation cured by heat alone.
Brekingsindex-bereikn = 1.45–1.50
1.162.00
ChemiefamilieThermal-curable latex
UithardingstypeThermal
ProductblokKM-001–040
Specificaties
Functies
Hard coatingAntifoulingAntistatic
Compatibele substraten
GlassPCPMMA
Verwerkingsmethoden
SPINDIPSPRAY
Brekingsindex-bereik
1.45–1.50
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-015 |
| Chemiefamilie | Thermal-curable latex |
| Brekingsindex-bereik | 1.45–1.50 |
| Uithardingstype | Thermal |
| PFAS-status | PFAS-vrij verkrijgbaar · fluorinated version available on request |
| Functies | Hard coating, Antifouling, Antistatic |
| Compatibele substraten | Glass, PC, PMMA |
| Verwerking | SPIN, DIP, SPRAY |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.