Alle producten
KM-010PFAS-vrij verkrijgbaar
UV Protection
UV-absorbing hard coating that protects underlying substrates and optical components from UV-induced yellowing and degradation. Suitable for outdoor display covers and automotive applications requiring long-term weatherability.
Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040
Specificaties
Functies
UV protection
Compatibele substraten
PETPCPMMA
Verwerkingsmethoden
SPINDIPROLLGRAVURE
Brekingsindex-bereik
1.48–1.55
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-010 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.48–1.55 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | UV protection |
| Compatibele substraten | PET, PC, PMMA |
| Verwerking | SPIN, DIP, ROLL, GRAVURE |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.