Alle producten
KM-009PFAS-vrij verkrijgbaar
Antiglare
Anti-glare coating that diffuses specular reflection to reduce glare from ambient light sources. Tuneable haze levels for different display viewing conditions while maintaining image clarity and contrast.
Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040
Specificaties
Functies
Anti-glare
Compatibele substraten
PETPCPMMATACGlass
Verwerkingsmethoden
SPINDIPROLLGRAVURE
Brekingsindex-bereik
1.48–1.55
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-009 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.48–1.55 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | Anti-glare |
| Compatibele substraten | PET, PC, PMMA, TAC, Glass |
| Verwerking | SPIN, DIP, ROLL, GRAVURE |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.