Alle producten
KM-007PFAS-vrij verkrijgbaar

Antifouling + Antistatic

Combined antifouling and antistatic functionality in a single UV-curable layer. Delivers WCA >100° and surface resistivity in the 10⁹ range. Eliminates the need for separate coating steps, reducing processing cost and time.

Brekingsindex-bereikn = 1.45–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040

Specificaties

Functies

AntifoulingAntistatic

Compatibele substraten

PETPCTAC

Verwerkingsmethoden

SPINDIPROLLGRAVURE

Brekingsindex-bereik

1.45–1.55
1.162.00
EigenschapWaarde
ProductcodeKM-007
ChemiefamilieSolvent UV-curable hybrid
Brekingsindex-bereik1.45–1.55
UithardingstypeUV
PFAS-statusPFAS-vrij verkrijgbaar · fluorinated version available on request
FunctiesAntifouling, Antistatic
Compatibele substratenPET, PC, TAC
VerwerkingSPIN, DIP, ROLL, GRAVURE
ProductblokKM-001–040
BatchgroottesVanaf 40 kg monster tot productieschaal
Houdbaarheid6 maanden (ongeopend)
KwaliteitISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch.

Monster aanvragen

Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.