Alle producten
KM-006PFAS-vrij verkrijgbaar
High Refractive Index
High refractive index coating tuneable from RI 1.65 to 2.00 via sol-gel nanoparticle chemistry. Achieves pencil hardness up to 8H on glass substrates. Essential building block for multi-layer AR stacks, waveguide cores, and index-matching applications.
Brekingsindex-bereikn = 1.65–2.00
1.162.00
ChemiefamilieSolvent sol-gel
UithardingstypeThermal
ProductblokKM-001–040
Specificaties
Functies
High RI
Compatibele substraten
GlassPETPCPMMA
Verwerkingsmethoden
SPINDIPROLLSPRAY
Brekingsindex-bereik
1.65–2.00
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-006 |
| Chemiefamilie | Solvent sol-gel |
| Brekingsindex-bereik | 1.65–2.00 |
| Uithardingstype | Thermal |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | High RI |
| Compatibele substraten | Glass, PET, PC, PMMA |
| Verwerking | SPIN, DIP, ROLL, SPRAY |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde casestudies
Displays0.41%Haze (vs 0.68% incumbent)ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser filmOptical Components8HPencil hardness at RI 1.85Thermal HRI coating reaches RI > 1.8 and 8H pencil hardness on specialty glassDisplays<0.15%Residual reflectanceBroadband reflectance below 0.15% achieved on multi-layer AR stack
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.