Alle producten
KM-005PFAS-vrij verkrijgbaar
Low Refractive Index
Ultra-low refractive index coating reaching RI as low as 1.16 — the lowest available from any PFAS-free supplier globally. Overcoatable for multi-layer AR stacks. Proven to survive furnace tempering at 630°C and deliver 2.5–4.5× light guiding luminance improvement on glass substrates.
Brekingsindex-bereikn = 1.16–1.40
1.162.00
ChemiefamilieSolvent sol-gel
UithardingstypeThermal
ProductblokKM-001–040
Specificaties
Functies
Low RIAnti-reflective
Compatibele substraten
GlassPETPCTAC
Verwerkingsmethoden
SPINDIPROLLSPRAY
Brekingsindex-bereik
1.16–1.40
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-005 |
| Chemiefamilie | Solvent sol-gel |
| Brekingsindex-bereik | 1.16–1.40 |
| Uithardingstype | Thermal |
| PFAS-status | PFAS-vrij verkrijgbaar |
| Functies | Low RI, Anti-reflective |
| Compatibele substraten | Glass, PET, PC, TAC |
| Verwerking | SPIN, DIP, ROLL, SPRAY |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde casestudies
Displays0.41%Haze (vs 0.68% incumbent)ULR coating achieves 0.41% haze vs 0.68% incumbent on polariser filmArchitectural Glass4.5×Luminance improvementLRI coating survives 630°C tempering, delivers 2.5–4.5× light guiding gainDisplays<0.15%Residual reflectanceBroadband reflectance below 0.15% achieved on multi-layer AR stack
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.