Alle producten
KM-003PFAS-vrij verkrijgbaar
Antifouling
Antifouling coating available as a PFAS-free variant, with water contact angle exceeding 100°. Resists fingerprints and smudges while maintaining optical clarity. Functionalised HSiO₂ nanoparticles provide durable easy-clean properties without perfluorinated chemistry.
Brekingsindex-bereikn = 1.40–1.50
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040
Specificaties
Functies
AntifoulingAnti-smudge
Compatibele substraten
PETPCPMMATACGlass
Verwerkingsmethoden
SPINDIPROLLGRAVURE
Brekingsindex-bereik
1.40–1.50
1.162.00
| Eigenschap | Waarde |
|---|---|
| Productcode | KM-003 |
| Chemiefamilie | Solvent UV-curable hybrid |
| Brekingsindex-bereik | 1.40–1.50 |
| Uithardingstype | UV |
| PFAS-status | PFAS-vrij verkrijgbaar · fluorinated version available on request |
| Functies | Antifouling, Anti-smudge |
| Compatibele substraten | PET, PC, PMMA, TAC, Glass |
| Verwerking | SPIN, DIP, ROLL, GRAVURE |
| Productblok | KM-001–040 |
| Batchgroottes | Vanaf 40 kg monster tot productieschaal |
| Houdbaarheid | 6 maanden (ongeopend) |
| Kwaliteit | ISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch. |
Gerelateerde toepassingen
Gerelateerde casestudies
Displays — Foldable200kFold cycles passedSingle-layer hardcoat passes 200,000 fold cycles with PFAS-free anti-smudgeDisplays — ULR0.3×Reflection vs referenceARAF nanoparticle composition achieves 0.3× reference reflection levelDisplays — Foldable>100°Water contact angle (PFAS-free)PFAS-free flexible AR achieves WCA >100° with better retention than PFAS
Monster aanvragen
Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.