Alle producten
KM-002PFAS-vrij verkrijgbaar

Antistatic

UV-curable antistatic coating providing surface resistivity in the 10⁹ Ohm/sq range. Prevents dust attraction and electrostatic discharge damage on display films and optical components. Proven at production scale, including 500,000 kg supplied as sole global supplier for PDP colour-filter applications.

Brekingsindex-bereikn = 1.48–1.55
1.162.00
ChemiefamilieSolvent UV-curable hybrid
UithardingstypeUV
ProductblokKM-001–040

Specificaties

Functies

Antistatic

Compatibele substraten

PETPCTACGlass

Verwerkingsmethoden

SPINDIPROLLGRAVURESLOT DIE

Brekingsindex-bereik

1.48–1.55
1.162.00
EigenschapWaarde
ProductcodeKM-002
ChemiefamilieSolvent UV-curable hybrid
Brekingsindex-bereik1.48–1.55
UithardingstypeUV
PFAS-statusPFAS-vrij verkrijgbaar
FunctiesAntistatic
Compatibele substratenPET, PC, TAC, Glass
VerwerkingSPIN, DIP, ROLL, GRAVURE, SLOT DIE
ProductblokKM-001–040
BatchgroottesVanaf 40 kg monster tot productieschaal
Houdbaarheid6 maanden (ongeopend)
KwaliteitISO 9001:2015-gecertificeerd. Gefilterd op 0,8 µm. Tot 10 CTQ-parameters per batch.

Monster aanvragen

Beschikbaar vanaf 40 kg monsterpartijen. Elke batch gefilterd op 0,8 μm en getest op maximaal 10 CTQ-parameters.

Neem contact op