VR / MR headset — pancake optics
Pancake optics fold the light path between a 50/50 mirror and a reflective polarizer, so the lens can sit close to the display and the headset gets shorter. The price is stray light: every extra reflection at a lens or film surface can reach the eye as a ghost image. Anti-reflection on every air-facing surface is part of the optical design.
Volledige lagenlijst (10)
- AR, hard coat and easy-clean Eye-side lens surfaceK1
- Lens 2 Polymer or glass
- Reflective polarizer Laminated film
- Quarter-wave plate Laminated film
- AR on the film surface Facing the folded cavityK2
- AR on lens 1 Cavity sideK2
- Lens 1 with 50/50 mirror Partial mirror on the display-side surface
- AR on the display film Facing lens 1K3
- Circular polarizer on the display Polarizer + quarter-wave film
- Display Micro-OLED or LCD
Werkwijze
Versie 1 · voor het eerst gepubliceerdAnti-reflection on every film and lens surface that faces air, from the display to the eye.
Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.
- AR on the film and lens surfaces inside the cavity
Multi-layer AR, R < 0.15 %, applied roll-to-roll on the films.
Lagen: AR on the film surface · AR on lens 1 - AR on the display film
Light sent back to the display returns as a ghost of 0.25 × the reflectance it meets there: about 1 % of the image for a bare film surface, 0.04 % with R < 0.15 %.
Lagen: AR on the display film - AR, hard coat and easy-clean on the eye-side lens
Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.
Lagen: AR, hard coat and easy-clean
Publieke onderbouwing
Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — Textbook: multi-layer anti-reflection designs for the visible.
Blijft bij de apparaatmaker
Polarizer and wave-plate films, the partial mirror and the lens design.
Deze beschrijving is geen juridisch advies.
Referenties
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
Bijbehorende Kriya-pagina's
Hier gebruikte Kriya-tools
Schematisch, niet op schaal.