Sunglasses — polarized lens
A sunglass lens is dark by design: a category 3 lens passes 8 to 18 % of the light. That is exactly why its back surface matters. Light arriving from behind or from the side is not dimmed by the lens at all — the bare back surface mirrors about 5 % of it straight into the eye, which can rival the dimmed scene in front. An AR coating on the back surface removes that glare; the front needs a hard coat and an easy-clean layer.
Volledige lagenlijst (8)
- Easy-clean topcoat FrontK3
- Mirror or flash coating (optional) Vacuum · not Kriya
- Hard coat, front Index-matched to polycarbonateK1
- Polycarbonate sheet Protects the polarizing film
- Polarizing film Dyed, stretched PVA · heat-sensitive · not Kriya
- Polycarbonate sheet and lens body Tinted · n 1.59
- Hard coat, backK1
- Back-side anti-reflection Faces the eyeK2
Werkwijze
Versie 1 · voor het eerst gepubliceerdA UV-cured hard coat matched to polycarbonate, a wet AR on the back surface, an easy-clean layer on the front; no bake after moulding.
Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.
- UV-cured hard coat matched to polycarbonate
Index up to 1.65 (polycarbonate: 1.59). Cured by UV light, so the polarizing film sees no further heat.
Lagen: Hard coat, front · Hard coat, back - Wet AR on the back surface
Behind a 12 % lens a bare polycarbonate back surface adds glare worth 43 % of the scene; with R < 0.15 %, about 1 %.
Lagen: Back-side anti-reflection - Easy-clean top layer on the front
Water contact angle above 100° without fluorinated chemistry.
Lagen: Easy-clean topcoat
Publieke onderbouwing
Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.
- US 4,070,097 — Ophthalmic antireflection coatings with metal, dielectric, substrate, metal, dielectric in sequence — 1976: in spectacles the unwanted reflected light comes from the back of the lens; the eye-side coating is built for low reflection seen from the eye.
- US 5,165,992 — Hard coating film and optical elements having such coating film — 1991: high-index oxide particles in the hard coat suppress interference fringes on n 1.56 and n 1.60 lenses.
- US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993: spin-coated hard coat on plastic lenses, cured by ultraviolet light.
Blijft bij de apparaatmaker
Polarizing film, tint, mirror coating and lens moulding.
Deze beschrijving is geen juridisch advies.
Referenties
- ISO 12312-1:2022 Eye and face protection — Sunglasses and related eyewear — Part 1: Sunglasses for general use — filter categories by luminous transmittance; category 3 is 8–18 %
- US 5,165,992 — Hard coating film and optical elements having such coating film — 1991 filing: high-index oxide particles in the hard coat suppress interference fringes on high-index plastic lenses
- US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light
- US 4,070,097 — Ophthalmic antireflection coatings with metal, dielectric, substrate, metal, dielectric in sequence — 1976 filing: in spectacles the unwanted reflection comes from the back of the lens, so the eye-side coating is built for low reflection seen from the eye