Brillen

Safety glasses and visors

Polycarbonate that must stay clear in dust and daily wiping

Safety glasses and visors are polycarbonate, chosen for impact strength — and polycarbonate is soft and charges easily. The standards allow two optional marks on the lens that buyers look for: resistance to surface damage by fine particles, and resistance to fogging. The first is a hard coat. Dust that clings to a charged lens gets wiped across it, so a hard coat that also bleeds off charge protects itself.

OUTSIDEEYE SIDEEasy-clean topcoatOuter faceAntistatic hard coat, outer faceMark K: resistance to surface damage by fineparticlesPolycarbonate lens or visorn 1.59Hard coat, inner faceAnti-fog coating, inner faceMark N: resistance to fogging · not KriyaK2K1K1
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (5)
  1. Easy-clean topcoat Outer faceK2
  2. Antistatic hard coat, outer face Mark K: resistance to surface damage by fine particlesK1
  3. Polycarbonate lens or visor n 1.59
  4. Hard coat, inner faceK1
  5. Anti-fog coating, inner face Mark N: resistance to fogging · not Kriya

Werkwijze

Versie 1 · voor het eerst gepubliceerd

An antistatic hard coat on both faces and an easy-clean layer outside; the anti-fog layer inside is a different chemistry.

Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.

  1. Antistatic hard coat on both faces

    Pencil hardness 3H+ to 4H on polycarbonate; surface resistance 10⁶–10¹² Ω/sq.

    Lagen: Antistatic hard coat, outer face · Hard coat, inner face
  2. Easy-clean top layer on the outer face

    Water contact angle above 100° without fluorinated chemistry.

    Lagen: Easy-clean topcoat
  3. Anti-fog layer on the inner face

    Not Kriya. The hard coat underneath has to accept it.

    Lagen: Anti-fog coating, inner face

Publieke onderbouwing

Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.

Blijft bij de apparaatmaker

Lens or visor moulding, marking and certification.

Deze beschrijving is geen juridisch advies.

Referenties

  1. BSI white paper: Protective Eyewear suite of standards — BS EN ISO 16321-1, -2 and -3 — EN ISO 16321 replaces EN 166; optional requirements and lens marking
  2. US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998 patent: UV-curable transparent coating made antistatic with conductive tin-oxide powder, for substrates such as polycarbonate
  3. EP 0 232 033 — Transparent electrically conductive plastic molded articles — 1987 publication: transparent, abrasion-resistant antistatic coat with tin-oxide powder on plastic mouldings
  4. US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light

Schematisch, niet op schaal.