Displays & wearables

MicroLED display

Getting light out of high-index LED chips

Micro-LED chips are made of GaN (n ≈ 2.4). A bare chip surface reflects 17 % straight back even at normal incidence, and in a flat stack only light within 24.6° of the normal can ever reach the air. Stepping the index down in layers cuts the reflection losses; a high-index layer with a shaped surface — a microlens or texture — accepts a much wider cone from the chip and lets it out. An AR-coated cover keeps ambient reflections down.

VIEWER SIDEBACKPLANEAnti-reflection coatingLow index n 1.16–1.40 or multi-layer ARCover glassn 1.52Optical fill / adhesiveNot KriyaColour-conversion layerQuantum dots on blue LEDs (in colour-converteddesigns)High-index extraction layerGraded n 1.95 → 1.40, or imprinted high-indexmicrolenses / textureMicro-LED chipsGaN · n ≈ 2.4TFT backplaneNot KriyaSubstrateGlass or siliconK1K2
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (8)
  1. Anti-reflection coating Low index n 1.16–1.40 or multi-layer ARK1
  2. Cover glass n 1.52
  3. Optical fill / adhesive Not Kriya
  4. Colour-conversion layer Quantum dots on blue LEDs (in colour-converted designs)
  5. High-index extraction layer Graded n 1.95 → 1.40, or imprinted high-index microlenses / textureK2
  6. Micro-LED chips GaN · n ≈ 2.4
  7. TFT backplane Not Kriya
  8. Substrate Glass or silicon

Schematisch, niet op schaal.