Vlakke optica & beeldvorming
Metalens
A flat lens made of sub-wavelength pillars
A metalens replaces a curved lens with millions of nanopillars whose width sets the local phase delay. To cover a full 2π of phase at a practical height, the pillars need a high index against their surroundings. Imprinting them directly in a high-index nanocomposite replaces deposition and etching for every part; a low-index embedding layer makes them robust.
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (5)
- Low-index embedding layer Protects the pillars; can carry an AR or be bondedK1
- Nanopillars Imprinted high-index nanocompositeK2
- Residual layer Same resin as the pillarsK2
- Substrate Glass wafer · n ≈ 1.46–1.52
- Backside anti-reflection Low-index or multi-layer ARK3
Referenties
- G. Yoon et al., Single-step manufacturing of hierarchical dielectric metalens in the visible — Nat. Commun. 11, 2268 (2020)
- Scalable manufacturing of high-index atomic layer–polymer hybrid metasurfaces for metaphotonics in the visible — Nature Materials (2023)
- S. M. Kamali et al., Decoupling optical function and geometrical form using conformal flexible dielectric metasurfaces — Nat. Commun. 7, 11618 (2016), open access: silicon nano-posts embedded in a low-index polymer
- H. A. Macleod, Thin-Film Optical Filters, 3rd edition (2001), chapter 3: Antireflection coatings — multi-layer designs for the visible; sections 3.4 and 3.5: coatings with two zeros, and coatings for the visible and the infrared together · link: publisher page of the current edition
Schematisch, niet op schaal.