An LCD shapes light from the backlight between two polarizers. Kriya chemistry sits on the polarizer films — where hard coat, low reflection and antistatic decide contrast, durability and touch performance — and can keep light guided when backlight films are bonded together instead of stacked with air gaps.
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (14)
- Surface treatment on the front polarizer Hard coat + low-reflection AR (anti-glare option)K1
- Front polarizer TAC / PVA / TAC · n ≈ 1.48–1.50
- Pressure-sensitive adhesive Not Kriya
- Colour-filter glass n 1.52
- Liquid crystal n ≈ 1.5–1.7
- TFT array glass n 1.52
- Rear polarizer TAC / PVA / TAC
- Antistatic hard coat On the rear polarizer filmK2
- Reflective polarizer film Recycles the blocked polarization
- Prism films Brightness enhancement
- Diffuser film Not Kriya
- Low-index layer for bonded backlight films Replaces the air gap above the light guideK3
- Light-guide plate with edge LEDs PMMA (n 1.49) or glass · printed extraction dots
- Reflector film Not Kriya
Referenties
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
- US 5,834,549 — Transparent conductive coating composition and transparent antistatic molded article — 1998 patent: UV-curable transparent coating made antistatic with conductive tin-oxide powder, for substrates such as polycarbonate
- US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
Bijbehorende Kriya-pagina's
- kriya-materials.com/applications/displays
- kriya-materials.com/case-studies/ulr-polarizer-benchmark
- kriya-materials.com/case-studies/display-ar-coating
Hier gebruikte Kriya-tools
Schematisch, niet op schaal.