A HUD reflects an image off the windshield into the driver's view. Conventional HUDs use the s-polarised reflection from the inner glass surface and hide the second reflection, from the outer surface, with a wedge-shaped interlayer. p-polarised HUDs project close to the Brewster angle (≈ 57° for glass), where bare glass reflects little p-light, and use a reflecting layer inside the laminate instead. In both, the image leaves the HUD unit through a cover in the dashboard.

OUTSIDEHUD UNITOuter glassn 1.52PVB interlayern 1.48 · wedge-shaped for the HUD · ATO-loadedfor solar controlInner glassn 1.52CabinHUD cover lensPolycarbonate or glass · closes the dashboardapertureAspheric and fold mirrorsNot KriyaPicture-generation unitTFT-LCD, micromirror or laser scannerK1K2
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (6)
  1. Outer glass n 1.52
  2. PVB interlayer n 1.48 · wedge-shaped for the HUD · ATO-loaded for solar controlK1
  3. Inner glass n 1.52
  4. HUD cover lens Polycarbonate or glass · closes the dashboard apertureK2
  5. Aspheric and fold mirrors Not Kriya
  6. Picture-generation unit TFT-LCD, micromirror or laser scanner