Datacenter & fotonica
Co-packaged optics
Polymer waveguides between photonic chip and fibre
Co-packaged optics moves the optical engine next to the switch chip. Polymer waveguides on the package carry light between the photonic chip and the fibres and couple adiabatically to silicon-nitride waveguides on the chip. They are built like a coating stack — lower cladding, core, upper cladding — and cured with UV and heat, so the index of every layer has to be set precisely.
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (5)
- Upper cladding Low indexK1
- Waveguide cores Patterned by lithography or imprintK2
- Lower cladding Low indexK1
- Photonic chip with SiN tapers Coupling region: tapers under the polymer cores · not Kriya
- Package substrate or interposer Not Kriya
Referenties
- J. Van Asch et al., Low-Loss Integration of High-Density Polymer Waveguides with Silicon Photonics for Co-Packaged Optics — arXiv:2503.02712 (2025): adiabatic coupling between on-chip SiN and package-level polymer waveguides
- Y. Shen et al., Polymer Waveguides for Co-Packaged Optics — precise refractive-index control between core and cladding; propagation loss < 0.1 dB/cm at 850 nm
- Silicon photonics packaging with single-mode polymer waveguides — process: lower cladding, core, patterning, upper cladding; UV and thermal cure
Bijbehorende Kriya-pagina's
- kriya-materials.com/applications/nanoimprint-wafer-level-optics
- kriya-materials.com/applications/photonics-metalenses
Hier gebruikte Kriya-tools
Schematisch, niet op schaal.