Energie, gebouwen & landbouw
CIGS thin-film solar cell
Nanoimprinted moth-eye texture on the front contact
In a CIGS cell, sunlight enters through a transparent AZO front contact (n 1.913 at 633 nm). A sub-wavelength moth-eye texture, imprinted in a resin of almost the same index, grades the step from air into the cell: fewer photons are reflected and more generate current. This is Kriya's peer-reviewed nanoimprint result.
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (6)
- Moth-eye texture UV-nanoimprinted Kriya high-index resist · n 1.792 at 633 nmK1
- AZO front contact Transparent conductor · n 1.913 at 633 nm
- i-ZnO / CdS buffer Not Kriya
- CIGS absorber 0.85–2.0 µm in the study
- Molybdenum back contact Not Kriya
- Glass substrate Not Kriya
Referenties
Bijbehorende Kriya-pagina's
- kriya-materials.com/applications/nanoimprint-wafer-level-optics
- kriya-materials.com/applications/solar-energy
Hier gebruikte Kriya-tools
Schematisch, niet op schaal.