AR headset — curved visor combiner
The simplest see-through display projects the image from displays above the eyes onto a large curved visor. A semi-reflective coating on the inside of the visor sends the image to the eyes; the outside surface sends a second, shifted copy. On a visor this ghost is strong: the mirror is weak, so most of the light reaches the outer surface.
Volledige lagenlijst (5)
- Easy-clean top layer Outer faceK2
- Hard coat and AR, outer face Convex side of the visorK1
- Polycarbonate visor Injection-moulded · n 1.59
- Semi-reflective coating Even thickness over the inner face · about 40 % · vacuum dielectric stack, not Kriya
- Displays and lenses above the eyes Not Kriya
Werkwijze
Versie 1 · voor het eerst gepubliceerdHard coat, AR and easy-clean on the outer face; one mirror of even thickness on the inner face.
Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.
- Hard coat with AR on the outer face
Hard coat 3H+ to 4H; two-layer UV-curable AR on polycarbonate, high index ≈ 1.75 under low index ≈ 1.30. Behind a 40 % mirror the ghost falls from 4.6 % of the image to 0.9 % at R = 1 % and 0.14 % at R < 0.15 %.
Lagen: Hard coat and AR, outer face - Easy-clean top layer
Water contact angle above 100° without fluorinated chemistry.
Lagen: Easy-clean top layer - Mirror of even thickness on the inner face
Vacuum coating over the whole face, about 40 %. Not Kriya.
Lagen: Semi-reflective coating
Publieke onderbouwing
Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.
- US 3,870,405 — Helmet sight visors — 1975: a visor with a partially reflective inner surface; the ghost image comes from its outer surface.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
Blijft bij de apparaatmaker
Mirror design and reflectance, visor shape and display optics.
Deze beschrijving is geen juridisch advies.
Referenties
- US 3,870,405 — Helmet sight visors — 1975 patent: visor with a partially reflective inner surface; the ghost image comes from the outer surface
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
Bijbehorende Kriya-pagina's
Hier gebruikte Kriya-tools
Schematisch, niet op schaal.