AR & VR

Smart glasses — laser scanning with a hologram in the lens

A projector in the temple, a holographic film inside a prescription lens

In laser-scanning glasses a small projector in the temple sweeps red, green and blue laser beams across the lens. A hologram inside the lens — a film a few tens of micrometres thick — diffracts the beams into the pupil while the rest of the lens looks like an ordinary prescription lens. The hologram does not survive heat, and the lasers hit the eye-side surface at a steep angle. Both facts decide which coatings can be used.

WORLD SIDEEYE SIDEHard coat, AR and easy-cleanWorld sideLens body, world sideLens polymerHologram film inside the lensEmbedded by the lens maker · photopolymer,stable to 60–120 °C · not KriyaLens body, eye sideCarries the prescription surfaceHard coat and angle-tuned AREye side: first surface the laser meetsK1K1K2
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (5)
  1. Hard coat, AR and easy-clean World sideK1
  2. Lens body, world side Lens polymer
  3. Hologram film inside the lens Embedded by the lens maker · photopolymer, stable to 60–120 °C · not Kriya
  4. Lens body, eye side Carries the prescription surface
  5. Hard coat and angle-tuned AR Eye side: first surface the laser meetsK1 · K2

Werkwijze

Versie 1 · voor het eerst gepubliceerd

Everything is applied to the finished lens and cured by UV light, below the hologram's temperature limit.

Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.

  1. UV-cured hard coat on both faces

    Cured by UV light, so the lens stays below the hologram's limit of 60–120 °C. Pencil hardness 3H+ to 4H.

    Lagen: Hard coat, AR and easy-clean · Hard coat and angle-tuned AR
  2. Low-index layer tuned to the laser's angle, eye side

    n 1.30, about 134 nm for 520 nm at 60°: s-polarised reflection falls from 21 % to 2.8 %; with n 1.20, to 0.02 % (thin-film model).

    Lagen: Hard coat and angle-tuned AR
  3. AR and easy-clean on the world side

    Multi-layer AR, R < 0.15 %; water contact angle above 100° without fluorinated chemistry.

    Lagen: Hard coat, AR and easy-clean

Publieke onderbouwing

Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.

Blijft bij de apparaatmaker

The hologram, the way it is embedded in the lens, and the projector.

Deze beschrijving is geen juridisch advies.

Referenties

  1. US 8,432,624 — Optical article and method for producing the same — fringes from index mismatch and thickness variation on n 1.67 and 1.74 lenses; oven cure at 125 °C
  2. US 5,246,728 — Scratch-resistant coating and method of making coated lenses — 1993 patent: spin-coated hard coat on plastic ophthalmic lenses, cured by ultraviolet light
  3. US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids

Schematisch, niet op schaal.