AR & VR

AR glasses — reflective waveguide

Glass plate with embedded partial mirrors, between bonded cover plates

A reflective waveguide carries the image inside a glass plate by total internal reflection and couples it out with a row of embedded, partially reflective surfaces. The plate guides only while its faces meet something of much lower index. Bond a cover plate straight onto it and the image leaks into the cover. A low-index coating between plate and cover keeps the light guided without an air gap; the lower its index, the more field of view survives.

WORLD SIDEEYE SIDEHard coat, AR and easy-cleanOn the world-side coverWorld-side cover plateFlat glass or polymer · n ≈ 1.5Optical adhesiveNot KriyaLow-index layerA few µm · n ≈ 1.2–1.25Glass waveguide with partial mirrorsn ≈ 1.5–1.8 · embedded reflective surfaces ·not KriyaLow-index layerA few µm · n ≈ 1.2–1.25Optical adhesiveNot KriyaEye-side cover plateFlat · a prescription lens stays a separatepartHard coat and multi-layer AREye sideK1K2K2K1
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (9)
  1. Hard coat, AR and easy-clean On the world-side coverK1
  2. World-side cover plate Flat glass or polymer · n ≈ 1.5
  3. Optical adhesive Not Kriya
  4. Low-index layer A few µm · n ≈ 1.2–1.25K2
  5. Glass waveguide with partial mirrors n ≈ 1.5–1.8 · embedded reflective surfaces · not Kriya
  6. Low-index layer A few µm · n ≈ 1.2–1.25K2
  7. Optical adhesive Not Kriya
  8. Eye-side cover plate Flat · a prescription lens stays a separate part
  9. Hard coat and multi-layer AR Eye sideK1

Werkwijze

Versie 1 · voor het eerst gepubliceerd

A low-index layer on both guiding faces, flat cover plates bonded over it, coated outer faces.

Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.

  1. Coat both guiding faces with a low-index layer

    n 1.20–1.25, 1 µm or more: a ray 5° beyond the critical angle reaches only about 0.1 µm into the layer. Against n 1.20 an n 1.60 plate guides beyond 48.6°.

    Lagen: Low-index layer
  2. Bond flat cover plates over it

    With the low-index layer in between, the index of the adhesive no longer matters. Adhesive and covers are not Kriya.

    Lagen: Optical adhesive · World-side cover plate · Eye-side cover plate
  3. Coat the outer faces

    Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.

    Lagen: Hard coat, AR and easy-clean · Hard coat and multi-layer AR

Publieke onderbouwing

Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.

Blijft bij de apparaatmaker

The plate with its partial mirrors, the coupling prism, and the prescription lens, which stays a separate part.

Deze beschrijving is geen juridisch advies.

Referenties

  1. US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
  2. EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder