AR & VR

AR glasses — holographic waveguide

Volume gratings in a thin film between two substrates

A holographic waveguide couples light in and out with volume gratings recorded in a photopolymer or liquid-crystal layer only a few micrometres thick. The substrates around it can be thin glass or plastic of ordinary index, so the range of guided angles is narrow from the start. Every layer added outside the guide — a cover, a second colour plate, a laminate — has to be separated from it by something of very low index.

WORLD SIDEEYE SIDEHard coat, AR and easy-cleanOn the world-side coverWorld-side coverBonded with optical adhesive · not KriyaLow-index layer0.5–2 µm · n ≈ 1.2SubstrateGlass or polymer, 50–500 µm · n ≈ 1.52Holographic grating layerPhotopolymer or liquid-crystal polymer, 2–5 µm· not KriyaSubstrateGlass or polymerLow-index layer0.5–2 µm · n ≈ 1.2Eye-side cover plateBonded with optical adhesive · not KriyaHard coat and multi-layer AREye sideK1K2K2K1
Gepubliceerde Kriya-positiePassend geplaatste Kriya-positieOverige laag
Volledige lagenlijst (9)
  1. Hard coat, AR and easy-clean On the world-side coverK1
  2. World-side cover Bonded with optical adhesive · not Kriya
  3. Low-index layer 0.5–2 µm · n ≈ 1.2K2
  4. Substrate Glass or polymer, 50–500 µm · n ≈ 1.52
  5. Holographic grating layer Photopolymer or liquid-crystal polymer, 2–5 µm · not Kriya
  6. Substrate Glass or polymer
  7. Low-index layer 0.5–2 µm · n ≈ 1.2K2
  8. Eye-side cover plate Bonded with optical adhesive · not Kriya
  9. Hard coat and multi-layer AR Eye sideK1

Werkwijze

Versie 1 · voor het eerst gepubliceerd

A low-index layer on both outer faces of the guide, flat covers bonded over it, coated outer faces.

Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.

  1. Coat both outer faces of the guide with a low-index layer

    n about 1.2, 0.5–2 µm. Against n 1.20 an n 1.52 guide guides beyond 52.1°. For polymer substrates: n 1.21 with an 80 °C cure, UV-curable from n 1.30.

    Lagen: Low-index layer
  2. Bond flat covers over it

    Optical adhesive on the low-index layer. Adhesive and covers are not Kriya.

    Lagen: World-side cover · Eye-side cover plate
  3. Coat the outer faces

    Hard coat (3H+ to 4H), multi-layer AR (R < 0.15 %) and an easy-clean top layer with a water contact angle above 100° without fluorinated chemistry.

    Lagen: Hard coat, AR and easy-clean · Hard coat and multi-layer AR

Publieke onderbouwing

Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.

Blijft bij de apparaatmaker

The grating layer, its recording and the layout of the guide.

Deze beschrijving is geen juridisch advies.

Referenties

  1. B. Kress, Optical waveguide combiners for AR headsets: features and limitations — Proc. SPIE 11062, 110620J (2019)
  2. US 6,742,921 — Light pipe, plate light source unit and reflection type liquid-crystal display device — 2000 priority: a layer bonded to a light guide through a lower-index layer, so that guided light is totally reflected at the interface
  3. EP 1 447 433 — Coating material composition and article having coating film formed therewith — 2001 filing: low-index coating from fine hollow particles in a binder

Schematisch, niet op schaal.