AR glasses — birdbath optics
In a birdbath module the image from a micro-OLED display is folded by a flat beamsplitter and a curved, partially reflective mirror in front of the eye. The optics are simple and the image is sharp, but the light meets a half-mirror three times, and every surface that carries no mirror adds a faint copy of the image next to the real one. Those second surfaces are where anti-reflection coatings earn their place.
Volledige lagenlijst (9)
- Hard coat and easy-clean Outer face of the shieldK1
- Front shield Tinted polycarbonate
- AR, inner face of the shieldK2
- AR on the mirror's convex side World-facing second surfaceK2
- Curved half-mirror 50–70 % reflective on the concave side · mirror coating not Kriya
- AR on the beamsplitter's second surface Eye-facing sideK2
- Beamsplitter 40–60 % reflective · not Kriya
- AR on the display cover and relay lensK3
- Micro-OLED display Above the beamsplitter · not Kriya
Werkwijze
Versie 1 · voor het eerst gepubliceerdAnti-reflection on every surface that carries no mirror, a hard coat on the shield.
Hoe deze coating wordt aangebracht — stappen, publieke onderbouwing en wat bij de apparaatmaker blijft.
- AR on the uncoated second surfaces
Convex side of the curved mirror and eye-facing side of the beamsplitter. Behind a 50 % mirror the ghost falls from 1.9 % of the image (bare PMMA) to 0.08 % with R < 0.15 %.
Lagen: AR on the mirror's convex side · AR on the beamsplitter's second surface - Shield: AR inside, hard coat and easy-clean outside
Hard coat 3H+ to 4H on polycarbonate; easy-clean with a water contact angle above 100° without fluorinated chemistry.
Lagen: AR, inner face of the shield · Hard coat and easy-clean - AR on the display cover and relay lens
Multi-layer AR, R < 0.15 %.
Lagen: AR on the display cover and relay lens
Publieke onderbouwing
Geselecteerde vervallen octrooien, publicaties, boeken en normen die de stand van de techniek beschrijven.
- US 3,870,405 — Helmet sight visors — 1975: a visor with a partially reflective inner surface; the ghost image comes from its outer surface.
- US 6,210,858 — Anti-reflection film and display device using the same — 1997: wet-coated AR built from a hard coat, a high-index layer and a low-index layer.
Blijft bij de apparaatmaker
Mirror and beamsplitter coatings, polarization films and the optical layout.
Deze beschrijving is geen juridisch advies.
Referenties
- US 3,870,405 — Helmet sight visors — 1975 patent: visor with a partially reflective inner surface; the ghost image comes from the outer surface
- US 6,210,858 — Anti-reflection film and display device using the same — 1997 filing: wet-coated anti-reflection film with hard coat, high-index layer and a low-index layer (n 1.20–1.55) that owes its index to micro voids
Bijbehorende Kriya-pagina's
Hier gebruikte Kriya-tools
Schematisch, niet op schaal.